STRONG die casting mould steel out of the "boundary" to get "good results"

STRONG die casting mould steel out of the "boundary" to get "good results"

  • Categories:News
  • Author:
  • Origin:
  • Time of issue:2021-11-15
  • Views:640

(Summary description)Before determining the feeding scheme of the mould, we must "get out" and get rid of the "bondage" to see clearly and comprehensively and get the correct results. Jump out of the "boundary" to get the "right result"!

STRONG die casting mould steel out of the "boundary" to get "good results"

(Summary description)Before determining the feeding scheme of the mould, we must "get out" and get rid of the "bondage" to see clearly and comprehensively and get the correct results. Jump out of the "boundary" to get the "right result"!

  • Categories:News
  • Author:
  • Origin:
  • Time of issue:2021-11-15
  • Views:640
Information

-- Determination of feeding scheme for die casting mould

Author: Li Zelin (Senior die casting mould consultant of STRONG)

When designing the feeding scheme of mould, try to get rid of the bondage of "intuition" or "inertia thinking". List all "possible" and "impossible" schemes for comprehensive analysis and comparison. Only in this way can we ensure to the maximum extent that the best scheme is adopted. In addition, it is definitely a good way to solve the problem of inexperience.

Example 1

1636703507207617.jpg1636703727434891.jpg1636703705416113.jpg

 

Scheme 1↓ 

004.jpg

 

Scheme 2

005.jpg

Scheme 3

006.jpg

 

It is difficult to avoid the aeration of the small plane in scheme 1, and the last filling of the hemispherical top in scheme 2. Only scheme 3, not only can avoid the above two situations completely, but also can control the whole filling state well. Therefore, after comparison and analysis, scheme 3 is the best.

 

007.jpg008.jpg009.jpg

——————————————————————————————————————————————————————————————————————————

 

Example 2

 

010.jpg011.jpg012.jpg

 

Scheme 1

013.jpg

 

Scheme 2

014.jpg

 

Scheme 3

015.jpg

 

Scheme 4 

016.jpg

 

Both scheme 1 and scheme 2 inevitably form aeration at the top of the boss. Both scheme 3 and scheme 4 can solve this problem. Compared with this two schemes, the process of scheme 3 is longer and the number of refractions is more. The flow of scheme 4 is short, the number of refractions is less, and the flow pattern is easy to control. Therefore, after comparison and analysis, scheme 4 is the best.

 

—————————————————————————————————————————————————————————————————————

 

Example 3

 

017.jpg018.jpg

 

Scheme 1 

 

019.jpg

 

Scheme 2 ↓

020.jpg

 

In scheme 1, the water inflow is too narrow and the flow rate is not enough to meet the filling requirements. The scheme 2 has very high requirements for the design of flow channel. If there is a slight deviation, there will be trapped gas. And the adjustable process space is limited. Therefore, both schemes are not ideal.

 

 

Scheme 3

021.jpg

 

Scheme 4 

022.jpg

 

The aisle in the middle of scheme 3 lengthens the filling process, which is not conducive to the transmission of pressure. When eddy current is generated on both sides of the product at last, it is impossible to eliminate die casting defects by increasing the pressure. Scheme 4 can solve these problems completely. Moreover, the structure is very compact. Therefore, after comparison and analysis, scheme 4 is the most reasonable.

 

023.jpg024.jpg025.jpg

—————————————————————————————————————————————————————————————————————

 

Example 4

026.jpg027.jpg028.jpg

 

Scheme 1

029.jpg030.jpg

 

Scheme 2 

031.jpg032.jpg

 

Scheme 3

033.jpg034.jpg

 

The biggest difficulty of this device is to solve the problem of filling on both sides of A and B, and to avoid gas trapping. In the scheme 3, a small slope is specially added to the feed liquid, which successfully solves the problem. And other solutions, even if added slope, also impossible to achieve. Therefore, the scheme 3 is the most reasonable.

035.jpg036.jpg037.jpg

———————————————————————————————————————————————————————————————————————————

 

Example 5

038.jpg039.jpg

040.jpg041.jpg

 

Before determining the feeding scheme of the mould, we must "get out" and get rid of the "bondage" to see clearly and comprehensively and get the correct results. Jump out of the "boundary" to get the "right result"!

Service hotline+86-0757-23322638

Websitehttp://en.strongmetal.cn/

AddressNo.32 Shizhou Industrial Zone, Chencun Town, Shunde District, Foshan City, Guangdong Province

Keyword:

Scan the QR code to read on your phone

Related News

There is currently no information to display
Please add data record on website background.

Official account

公众号二维码
这是描述信息

Online customer service hotline

Add:Shizhou, Chencun, Shunde, Foshan, Guangdong 528313, China
Tel:
0757-23322638
Fax:0757-23322619

Copyright © 2020 Guangdong Strong Metal Technology Co., Ltd  All Rights Reserved.  粤ICP备09051653号  Powered by www.300.cn